dear sir,
for casting & forging- standard test bar is enough for conducting mechanical testing
for plate - we can take mechanical test sepecimen size as per ASME sec IX sample picture
Regards,
Sankaran.SP
Welding & Metallurgy expert
Coimbatore, India.
On Saturday 28 December, 2024 at 11:14:09 pm IST, Chandrapal Singh <avioraio@gmail.com> wrote:
How to select sample size for mechanical testing for different material (casting , rolled plate forging)