[MW:35374] Re: Corrosion Rate criteria for material UNS N06022 nickel alloy

Corrosion Rate required based on the process fluid,
Client has to provide


On Monday, December 2, 2024 at 3:39:50 PM UTC+5:30 Vivek wrote:
Team,
This is regarding material UNS N06022.

The corrosion Test is carried out as per ASTM G28 Method A.
The test result is 37.762 mpy (0.9592 mm/year).

May I know which standard provides acceptance criteria (range) for corrosion rate?

Regards,
Vivek

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/d52f1938-345e-41a5-86a6-e82eefd10f18n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...