AC GTAW with water cooled torch & HF unit
Thanks & Regards may be suitable for sheet metal.
J.Gerald Jayakumar
0091-8838619635
On Thursday, 31 March, 2022, 04:16:04 pm IST, Prem Nautiyal <prem.nautiyal26@gmail.com> wrote:
Hi Anthony
You may please try with 99.9995% Ultra Pure Argon gas. Use a gas cup size of 20#.
Use the forehand technique in MIG.
MIG always works with DC, for GTAW you should go with AC.
Use a better quality branded filler wire spool.
Regards
Prem Nautiyal
Welding & NDT Specialist
Cell 9769316004
On Thu, 31 Mar 2022, 15:36 'james gerald' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
--Try AC currentThanks & Regards
J.Gerald Jayakumar
On Thursday, 31 March, 2022, 01:03:59 pm IST, Anthony Dalisay <anthonydalisay6@gmail.com> wrote:Dear experts,We have been welding aluminized sheet using MIG welder with the following parameters:Amps: 125Volts: 29.5TS: 50cm/minGas flow rate: 12L/minGas type : 18%CO2 and 82%ArHowever, I cant get rid of black soot (smoke) in the weld vicinity. What do you think, is the best way to do to achieve cleaner weld in aluminized sheet such as this?Refer to attached photo for reference.Thanks in advance for your expert advice.Regards,Anthony----Anthony Dipasupil DalisayTWI AWeldI
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALBzUBLiVBU2wnkd3MGhgAMdC%2BMzEjF4SXM%2BsdgMXQgp5MVh9Q%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1137188882.137058.1648720763794%40mail.yahoo.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEP2HKDay-8%2Be1ViPnRSb1--q7R5DGACFPVtccN7Fku7v9jA1A%40mail.gmail.com.
Comments