It is not required if code of construction and client specification doesnt write it anywere... no need of that

On Wed, 2 Mar 2022, 7:17 am anthony chundal, <anthony.chundal@gmail.com> wrote:
It is required for service requirements, even though there is no welding

On Mon, 28 Feb 2022, 12:33 Muhammed Ibrahim PK, <ibratech@gmail.com> wrote:
Gentlemen,

Please advice PWHT required or not for small blind flanges also if the vessel is in sour service.The blinds having no welding on it.

As per my understanding PWHT is only for weld, not for base metal.

If welding on blinds like davit, manway handle can be justified. Is it required for other blinds not having any weld on it.

Experts please provide your view on it.


Reg,
Ibrahim

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALOPgmOMLrK_C5nWBaLNRqTSfCd24jm76qDB%2B0EoOoXk7J%3Dayw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOi%3DZp-LN3f20xe1kJKXj0EE-gFRuxH136JVEe%3D0X1Kh87iYhg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOWr6k-3_RNco3eNU-BXvwTmA%3DHoSd0g%3Dt4bicfPTi4MAxUu6g%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...