Also during shop & site Hydro Test.
Thanks & Regards
J.Gerald Jayakumar
On Tuesday, 1 March, 2022, 07:30:16 am GMT+4, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Normally I suppose vessel Blind Flanges are for temporary till transportation to site and moreover it shall meet the material standard as per Drawing or Design data sheet via a MTC.
Thanks & Regards
J.Gerald Jayakumar
On Monday, 28 February, 2022, 12:33:30 pm GMT+4, Muhammed Ibrahim PK <ibratech@gmail.com> wrote:
Gentlemen,
-- Please advice PWHT required or not for small blind flanges also if the vessel is in sour service.The blinds having no welding on it.
As per my understanding PWHT is only for weld, not for base metal.
If welding on blinds like davit, manway handle can be justified. Is it required for other blinds not having any weld on it.
Experts please provide your view on it.
Reg,
Ibrahim
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALOPgmOMLrK_C5nWBaLNRqTSfCd24jm76qDB%2B0EoOoXk7J%3Dayw%40mail.gmail.com.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1376188266.1672364.1646044807559%40mail.yahoo.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1376188266.1672364.1646044807559%40mail.yahoo.com.
Comments