Re: [MW:32997] PPM to mg/m2 conversion

1% is 10000 ppm and it must be 20ppm, please check

Thanks & Regards

J.Gerald Jayakumar



On Monday, 28 March, 2022, 07:14:50 am GMT+4, Muhammed Ibrahim PK <ibratech@gmail.com> wrote:


Gents,

Is there any conversion available for ppm to mg/m2?

For Aramco projects, the chloride content measured in ppm using bresle patch kit in ppm.

As per Aramco spec the acceptable range is 20mg/m2.

Couldn't find the conversion. If anybody can advice, it will ne highly appreciated

Reg,
Ibrahim

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALOPgmNqFyBdfAsrXAfykfbe4-Yw%2B0hZHYxmrDWA8uHC5WUiow%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...