Re: [MW:32953] What is difference between LST and MDMT

MDMT is taken in a Totality the lowest temperature attained either due to Environment, Service temperature, upset conditions etc..

Thanks & Regards

J.Gerald Jayakumar




On Thursday, 3 March, 2022, 12:33:14 pm GMT+4, SN <suryawanshinileshj@gmail.com> wrote:


Dear all,

Can you please explain 

What is the difference between MDMT and LST

Is MDMT(Minimum Metal Design Temperature ) and LST(Lowest Service Temperature) is same.

This concept is applicable  the exemption of Impact test requirements  as per UCS 66 and section III NF

Kindly clarify

Thanks.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CALi4c7Mpj1g5PLwBD%3D7fyWPrw3SnvpDAoAJX3vM6GRne0Lz%2BDA%40mail.gmail.com
.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...