Thursday, March 3, 2022

Re: [MW:32952] WPQ of single process having combination PQR

Yes you do

Στις Σάβ 26 Φεβ 2022 στις 6:08 π.μ., ο/η Brijesh Maurya <brijeshmaurya492@gmail.com> έγραψε:
Dear All,
I have PQR of GTAW + SMAW process for P1G2 to P1G2 (SA516 GR.70 to SA516 GR.70)
PQR Plate thickness = 10 mm
GTAW welded = 4 mm
SMAW welded = 6 mm
WPS range qualified = 1.5 to 20 mm.

Now, My query is, can i use this WPS for WPQ by GTAW process only?
I want to qualify my welder on 1/2"NB X SCH 160 (4.78 THK) pipe with only GTAW process using this WPS.

Kindly Clarify Experts........


Regards,
Brijesh Maurya

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOBi_eMeAVHXjg29UVz9HjnkscfsZX9-0hGMc-rOZCqWsA1C_A%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40CxeMKnwPkEsrfTzau94mUhr8-dkNjSe5D6oCYEv1vRGg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...