Can anyone share WPS for P11-335 to SS321 OR SS316

On Thursday, March 20, 2014 at 3:41:35 PM UTC+5:30 Azam Mohd wrote:

Use below filler wire and electrode, Having good weldability. We have qualified PQR with this consumable:

ERNiCr-3/ ENiCrFe-3




On Wed, Mar 19, 2014 at 4:05 PM, Ganesh Mahankal <mahan...@gmail.com> wrote:
 
Dear All ,
 
Is P11 to Stainless Steel(304L or 316L) welding possible?
 
If yes then plz mention by which welding consumables?
 
Best Regards,
 
Ganesh Mahankal
Alfa Laval India Ltd.Pune India
 

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/46406915-0ae0-486a-a7ad-088a9d38769fn%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...