Thursday, September 30, 2021

[MW:32541] Acceptance criteria for distortion

Dear Expert

Can some help to get the distortion acceptance criteria to WQT at 4G position.

--

--
Best Regards
Samiulla Syed,
Senior Trainer,
Welding Department,
TUV Rheinland Arabia LLC
National Industrial Training Institute,
Al Ahsa,
Eastern Province,
Kingdom of Saudi Arabia,
Email: ssyed@niti.edu.sa
          qcsyedsami@gmail.com
Mobile: +966(0)595531593.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFRNJK8xjqNeVZqH8mPSiJXiGOeyRarkk%3Dj3qytygKrBKVVRMA%40mail.gmail.com.

Re: [MW:32540] change in sfa number

There are 3 points to be considered as experts mentioned as below.

1. In ASME 2021 edition SFA 5.36 has been discontinued but I suppose the recalled may be used based provided the welding consumable certificate matches with A-Number of that Qualified for PQR.
 
2. Both SFA 5.20 & SFA 5.36 falls under F-Number 6 & hence  no issue.

3. Ensure the Shielding gas as qualified for 100%Co2

Thanks & Regards

J.Gerald Jayakumar



On Thursday, 30 September, 2021, 08:51:15 am IST, Chaudhary Zafar Iqbal <chzaiqbal88@gmail.com> wrote:


Hello good evening all experts
Can we use E71T1-1C-H4/H8 AWS SFA 5.36 filler wire instead of E71T1-1C-H4/H8 AWS SFA 5.20 if yes then please send me any  reference from code and standard by ASME-2C or SEX 9 or SAES- W12 or W11 or any international standard because our WPS is qualified on AWS 5.20 but we recieved Consumable material AWS SFA 5.36.         This attached label is recieved material 

Regards ,
Zafar 
00966544639978 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP9k9XfupDcLPwdc9kiJyUMxaU%2Bhz%3DHr13PVMmsgj_bO%3Dy_OEw%40mail.gmail.com.

Re: [MW:32538] change in sfa number

SFA no is not essential, only Fno & Ano is essential

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Thu, Sep 30, 2021 at 8:51 AM Chaudhary Zafar Iqbal <chzaiqbal88@gmail.com> wrote:
Hello good evening all experts
Can we use E71T1-1C-H4/H8 AWS SFA 5.36 filler wire instead of E71T1-1C-H4/H8 AWS SFA 5.20 if yes then please send me any  reference from code and standard by ASME-2C or SEX 9 or SAES- W12 or W11 or any international standard because our WPS is qualified on AWS 5.20 but we recieved Consumable material AWS SFA 5.36.         This attached label is recieved material 

Regards ,
Zafar 
00966544639978 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP9k9XfupDcLPwdc9kiJyUMxaU%2Bhz%3DHr13PVMmsgj_bO%3Dy_OEw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNvjT6LLE6R8TFyPw1EbZfBY_uS21dhtadb4xDsqtLkDA%40mail.gmail.com.

[MW:32537] Cladding consumable regd


Hello experts. 

Can u pls advise me laser cladding powder  on 1.4113 (X3CrNi) substrate ?  

Clad layer is specified 32 to 35 HRC hardness 

Thanks

Neilashkumar P 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/95155926.475400.1632975972041%40mail.yahoo.com.

Wednesday, September 29, 2021

[MW:32534] change in sfa number

Hello good evening all experts
Can we use E71T1-1C-H4/H8 AWS SFA 5.36 filler wire instead of E71T1-1C-H4/H8 AWS SFA 5.20 if yes then please send me any  reference from code and standard by ASME-2C or SEX 9 or SAES- W12 or W11 or any international standard because our WPS is qualified on AWS 5.20 but we recieved Consumable material AWS SFA 5.36.         This attached label is recieved material 

Regards ,
Zafar 
00966544639978 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP9k9XfupDcLPwdc9kiJyUMxaU%2Bhz%3DHr13PVMmsgj_bO%3Dy_OEw%40mail.gmail.com.

[MW:32533] Re: Is P11 to Satainless Steel(304L or 316L) welding possible?

Dear Ganesh 

The compatible filler metal shall be decided based on 
1) Service temperature 
2) Type of butt joint - Butt/ fillet 
3) PWHT required or not 
4)Service type -Elevated/corrosion  etc

Pl. state all the requirements from drawing/specs   then we experts can give suitable advice 

Vishwas 
9823472273 
Head - Welding Technology
On Wednesday, March 19, 2014 at 6:35:37 PM UTC+5:30 mahan...@gmail.com wrote:
 
Dear All ,
 
Is P11 to Stainless Steel(304L or 316L) welding possible?
 
If yes then plz mention by which welding consumables?
 
Best Regards,
 
Ganesh Mahankal
Alfa Laval India Ltd.Pune India
 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a84d70bc-223d-4f1c-859f-48452bd7a321n%40googlegroups.com.

Re: [MW:32532] Fabrication of Tanks in the Cold countries with Ambient temperature of -40 deg. C

Please see the requirements for ASME Sec VIII Div-I snap shot on lowest temperature during welding.

Inline image

Please check the particular Design and Fabrication Code and specification for the minimum permissible temperature and take action accordingly.

Thanks & Regards

J.Gerald Jayakumar



On Wednesday, 29 September, 2021, 08:45:53 am IST, N VENKATESWARA PRASAD <weldengr.velosi@gmail.com> wrote:


Dear All,

What are the precautions required to fabricate the Tanks of ASTM A 537 cl1 of thickness varies from 8-20mm with 6 to 10 m height. What are the precautions required.  If any one is having this experience, please provide your contact details.  I will contact you.

Regards

N.V. PRASAD
+968 98511695 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL%3D4YYiYcaWxTi8TDo_36HzuJaPCTCW_O%3D_W89WoD_W8C_sD-Q%40mail.gmail.com.

[MW:32531] Usage of Rebar at Pipe Gap


Dear Experts,

I am currently working in a project which follows AWS standard.The welding design is a butt weld followed by fillet welds.Can I use rebar to fill the gap for the butt weld?. If so ,Can you please refer me to the code which allows or doesn't allow the use of rebar to fill up the gap before welding.

Thank you

The information contained in this e-mail may be privileged and confidential. If the reader is not the intended recipient, or agent of the intended recipient, any unauthorised use, disclosure, copying, distribution or dissemination is strictly prohibited. If you have received this communication in error, please notify the sender immediately and delete it from your system.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2896d687-f883-4d80-ba6f-f59e58ad71d7n%40googlegroups.com.

Tuesday, September 28, 2021

[MW:32529] Fabrication of Tanks in the Cold countries with Ambient temperature of -40 deg. C

Dear All,

What are the precautions required to fabricate the Tanks of ASTM A 537 cl1 of thickness varies from 8-20mm with 6 to 10 m height. What are the precautions required.  If any one is having this experience, please provide your contact details.  I will contact you.

Regards

N.V. PRASAD
+968 98511695 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL%3D4YYiYcaWxTi8TDo_36HzuJaPCTCW_O%3D_W89WoD_W8C_sD-Q%40mail.gmail.com.

Re: [MW:32529] Is P11 to Satainless Steel(304L or 316L) welding possible?

Can anyone share WPS for P11-335 to SS321 OR SS316

On Thursday, March 20, 2014 at 3:41:35 PM UTC+5:30 Azam Mohd wrote:

Use below filler wire and electrode, Having good weldability. We have qualified PQR with this consumable:

ERNiCr-3/ ENiCrFe-3




On Wed, Mar 19, 2014 at 4:05 PM, Ganesh Mahankal <mahan...@gmail.com> wrote:
 
Dear All ,
 
Is P11 to Stainless Steel(304L or 316L) welding possible?
 
If yes then plz mention by which welding consumables?
 
Best Regards,
 
Ganesh Mahankal
Alfa Laval India Ltd.Pune India
 

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/46406915-0ae0-486a-a7ad-088a9d38769fn%40googlegroups.com.

Monday, September 27, 2021

[MW:32528] Essential variables for Welding Procedure as per API 1104 22nd edition

Greetings,
As per Latest's edition of API 1104 (22nd edition) Table 1 Essential variables for qualification of welding procedure Specifications, Diameters are not listed as a essential variables.
Please share your experiences with standard references for diameter of Pipe are essential variables or not as per API 1104?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/C7F16A03-1358-4AE6-AD80-9A69B0878B61%40gmail.com.

Re: [MW:32526] PQR-Qualified in Duplex Stainless Steel UNS-31803 / WPS-UNS-32750

There are certain points to be considered.

1. Though both UNS-31803 & 32750 falls under same P-No: 10H / 1 but their UTS values are different. UNS 31803 welded using consumable ER 2209 which produces a UTS value of 90ksi whereas UNS32750 shall be welded with a consumable which has a UTS valiue of 120Ksi and hence preferred ER2594.

2. ASTM G48 tests are mandatory to ascertain its suitability to service, UNS31803 tested at temperature of 25degC whereas UNS 32750 tested at  40dgeC and hence suitable welding consumable to be selected.

3. Generally welds are considered anodic when compared with the Basemetal due to its area and corrosion are localized in welds. UNS 31803 has a PREN value of 34 whereas UNS 32760 has a PREN value of 40 due to its high alloy elements.

4. Moreover for Duplex and superduplex stainless steels are governed by various Clients specifications which will be more demanding and will not permit.

Hence WPS for UNS31803 cannot be used for UNS32750.

Hope our experts can add more points to clarify.

Thanks & Regards

J.Gerald Jayakumar



On Monday, 27 September, 2021, 08:42:20 am IST, Muhammad Azeem <azeem7999@gmail.com> wrote:


Gents,
I need your kind reference comments to clarify regarding the separate WPS required for each UNS in P-10H qualification ..
If PQR qualified with UNS-31803 Duplex Stainless Steel.
WPS can be prepared with UNS-32750 Super Duplex Stainless ...



Regards,

Muhammad Azeem Iqbal

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f8e9def5-aaca-41f7-9d07-abc3d1836bd3n%40googlegroups.com.

[MW:32525] RE: PQR-Qualified in Duplex Stainless Steel UNS-31803 / WPS-UNS-32750

No, in most of the cases.

32750 is a SDSS(25Cr), while 31803 is a DSS(22Cr). For P10H group every grade is different, in chemistry, mechanical properties & corrosion resistance. You require separate PQR with all comprehensive testing for each individual grade.

 

What're the process requirements and intended service/s.

 

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent  Welding & Metallurgical Engineering Specialist

Consultant: SNC Lavalin Inc. (Nuclear &Non-Nuclear)

Saudi Aramco Approved Designated Project Welding Engineer (DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

From: Muhammad Azeem <azeem7999@gmail.com>
Sent: September 26, 2021 4:08 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: PQR-Qualified in Duplex Stainless Steel UNS-31803 / WPS-UNS-32750

 

Gents,

I need your kind reference comments to clarify regarding the separate WPS required for each UNS in P-10H qualification ..

If PQR qualified with UNS-31803 Duplex Stainless Steel.

WPS can be prepared with UNS-32750 Super Duplex Stainless ...

 

 

 

Regards,

 

Muhammad Azeem Iqbal

 


Virus-free. www.avg.com

Thursday, September 23, 2021

Re: [MW:32523] GOST GRADE

Below link software Total Materia contains the equivalent grades. Please check in our group anyone having access can help.


Thanks & Regards

J.Gerald Jayakumar




On Thursday, 23 September, 2021, 10:42:17 am IST, dpsh...@gmail.com <dpshaju1@gmail.com> wrote:


Hello

 Can anyone help me with equivalent ATSM grade for the below GOST grade

Ст20 &  16гс

Regards,

Saju Dayanandan

+91 9860627018 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/eaf5a176-68f2-401b-994c-f5905c1c2e47n%40googlegroups.com.

[MW:32522] Alternative to Drop weight test

Dear Gentlemen,

Is there any alternative to Drop Weight test (ASTM E 208) in any national or international standard ??

Request you feedback.

Regards,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALi4c7N3TfT56_Dd%3D0dbFjYYuMWtPjNQHyrw6-umxUmTFOaFdg%40mail.gmail.com.

Saturday, September 11, 2021

Re: [MW:32515] Cracking of Monel 400 TTS welds

Hi JP,
Monel being critical material from welding point of view, we have to take care of general good engineering practices like sequence of welding, proper shielding by inert gas, control of heat input, the gap (if any) between tube and tube sheets, etc. In sequence of welding try to weld the joint in multiple segments with sufficient overlaps from starting to end points. Many time the cracks develops due to minor things those are very critical to particular materials.

Thanks,
Best Regards,
Rajnish Dixit
On Monday, 30 August, 2021, 02:12:08 pm IST, Jeya Prakash <jeyaprakashjj@gmail.com> wrote:


Dear Experts,
We are facing cracking issues during welding in Monel 400 Tube to Tubesheet Joints. Refer attached photographs.
Tube: SB-163 UNS-N04400; 25.0 mm OD x 2.0 mm thk
Tubesheets: SA-336M Gr F304L + SB-127 UNS-N04400 (48 + 10 mm thick clad)
Welding: ERNiCu-7 GTAW filler wire with Ar shielding gas.
crack locations: weld toe on tube side, tube ends.

Kindly share the reason for such cracking, and precautions required during Monel 400 welding.

Thanks in Advance.

Regards,
Jeya Prakash. J

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL5WJhc%2BRkjr6oAUNp8uvhCP1imK0on-mqp7jbWcVAZC0PRy-Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1416330614.2749707.1631345653147%40mail.yahoo.com.

Thursday, September 9, 2021

Re: [MW:32514] Welding process and NDT method for fillet welding


Dear Sir,

Pipe Size .3/4 inch sch 160 (5.56 wall thk ) 

Used WPS for welding with pwht : Temp 720 degree plus minus 20 degree 
Soaking Time 2HR 25 MIN .

as per ASME B31.3  its exempted ..as thk is less than 16mm .

but if we used wps with pwht then its mandatory to do the PWHT ?

from B31.3 Table  331.1.3 exemption of pwht

any sabic spec saying about this ??

we have socket weld (fillet weld) and Goove weld to do PWHT ..

thanks in advance 

Further to above what is the calibration range for pressure gauges in SABIC ? any standard ? or any procedure .


Regards ,
Zafar 
Mob / whatsapp 00966544639978 

On Wed, 1 Sept 2021 at 14:50, 'SENTHILKUMAR SWAMINATHAN' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Magnetic Particle Testing (Wet ) or Dye Pen 

Thank you, 

Regards, 
S.SENTHILKUMAR


On Wednesday, 1 September, 2021, 08:36:00 am IST, Chiranjeevi A <chiranjeevipuvvula@gmail.com> wrote:



Dear Experts,

 

Please advice on NDT methods for fillet welding in plate welding (A36 mtl) for Ducts



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0xCpJmaGRR8QbY6JihPBAQbNDab%3D9Z%2BKqykWswmwNRZAg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/274539791.938607.1630471609411%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP9k9XfYCQzXw%3DeooZvR0bYix-sPii-_%2BHT7bMztdbCv6CEHkg%40mail.gmail.com.

[MW:32513] Regarding PWHT THICKNESS

Dear all,
         Pls I needs your all valuable comments regarding PWHT thickness,
As per ASME B31.3 2018 
,Table 331.1.1, whether PWHT based on thickness of base metal or P.No and Group No,
 I appreciate your guidance,
SENTHIL P





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGYkEe1qDTRTenRNue9n11VZPewmwR_K8NVT_jA%2BL%2BeCVNhDrg%40mail.gmail.com.

Wednesday, September 8, 2021

Re: [MW:32511] QT stamp on Quenched and Tempered forgings

Check your MTC for the type of Heat Treatment performed and take necessary action with the concurrence of your Client.

Thanks & Regards

J.Gerald Jayakumar



On Tuesday, 7 September, 2021, 10:18:06 am IST, vivek kb <vivekkb87@gmail.com> wrote:


Dear Experts,

Below is an excerpt from ASME SA-350 and is related to product marking:

image.png

Could you please advise the basis of this requirement. In most cases, this stamping is specified for Quenching and tempered or Quenching and precipitation heat treated only unlike the Normalizing or Normalized and tempered.

Regards,
Vivek.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB3WdPMJ0Rz4F0ZaRKJiFx_HkZbr%3DpNiOhtqKiMdEM6AA4%3DSwA%40mail.gmail.com.

Tuesday, September 7, 2021

Re: [MW:32510] QT stamp on Quenched and Tempered forgings

Toughness value will be  more than Normalizing, Welding related issues will be more in QT if proper procedure is not followed. 

On Tue, Sep 7, 2021, 10:18 AM vivek kb <vivekkb87@gmail.com> wrote:
Dear Experts,

Below is an excerpt from ASME SA-350 and is related to product marking:



Could you please advise the basis of this requirement. In most cases, this stamping is specified for Quenching and tempered or Quenching and precipitation heat treated only unlike the Normalizing or Normalized and tempered.

Regards,
Vivek.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB3WdPMJ0Rz4F0ZaRKJiFx_HkZbr%3DpNiOhtqKiMdEM6AA4%3DSwA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePHsJS0pYnNu0X6Z%3Dskw17%2B%2BDpCAgUkEXy%2B-srL_e2ZHA%40mail.gmail.com.

Monday, September 6, 2021

[MW:32509] QT stamp on Quenched and Tempered forgings

Dear Experts,

Below is an excerpt from ASME SA-350 and is related to product marking:



Could you please advise the basis of this requirement. In most cases, this stamping is specified for Quenching and tempered or Quenching and precipitation heat treated only unlike the Normalizing or Normalized and tempered.

Regards,
Vivek.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB3WdPMJ0Rz4F0ZaRKJiFx_HkZbr%3DpNiOhtqKiMdEM6AA4%3DSwA%40mail.gmail.com.

Friday, September 3, 2021

Re: [MW:32507] AWS WPS & WELDER QUALIFICATION

Dear sir, 
Please note that qualification for WPS and welder are deference
For welder, he can weld F, H, V but PQR/ WPS must be qulified more 
Vào Th 5, 2 thg 9, 2021 lúc 10:37 Vishwas Keskar <vvkeskar123@gmail.com> đã viết:
AWS Table  is very clear for WPS PQR.
For each position ,PQR is needed .

Qualify PQR positions based on  envising Production Welding Joint positions.

For Welder , range for Qualified position is given based on WPQ tested position.




On Wed, 1 Sep 2021, 17:20 DINESH KUMAR DEVENDHIRAN, <dineshqc05@gmail.com> wrote:
Dear Experts
I need a clarification on AWS table 4.1 vs 4.10
As per table 4.1- for 3G position WPS shall be qualify for vertical position only
As per table 4.10 - for 3G position welder will qualify for Flat, Horizontal, vertical.

My doubt is if i have a WPS for 3G uphill position, can i use the same WPS for 1G&2G also ?
If not please explain.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/571704be-652c-417c-9c67-6400ec82034an%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3P7Fs6c5nxzvj3o8SABXy9ePm0VZdkkxQV2n84iCYgU7Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHTP-OmxfT5VF%3D6iDqtp%3DnCvh0_zLLHCTShPQdt8zqK5_7mrgg%40mail.gmail.com.

Thursday, September 2, 2021

Re: [MW:32506] AWS WPS & WELDER QUALIFICATION

AWS Table  is very clear for WPS PQR.
For each position ,PQR is needed .

Qualify PQR positions based on  envising Production Welding Joint positions.

For Welder , range for Qualified position is given based on WPQ tested position.




On Wed, 1 Sep 2021, 17:20 DINESH KUMAR DEVENDHIRAN, <dineshqc05@gmail.com> wrote:
Dear Experts
I need a clarification on AWS table 4.1 vs 4.10
As per table 4.1- for 3G position WPS shall be qualify for vertical position only
As per table 4.10 - for 3G position welder will qualify for Flat, Horizontal, vertical.

My doubt is if i have a WPS for 3G uphill position, can i use the same WPS for 1G&2G also ?
If not please explain.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/571704be-652c-417c-9c67-6400ec82034an%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3P7Fs6c5nxzvj3o8SABXy9ePm0VZdkkxQV2n84iCYgU7Q%40mail.gmail.com.

Wednesday, September 1, 2021

Re: [MW:32505] AWS WPS & WELDER QUALIFICATION

Hai,

If your welder tested in 3G Position he can weld F,H & V Position.

3G PQR Will support only Vertical Welding.

If you need F&H position you need to establish New pqr with 2G position.

Regards,
Manikandan
9791367960

On Wed, Sep 1, 2021, 9:03 PM Manikandan J <mechmani22@gmail.com> wrote:
Hai,

If your welder tested in 3G Position he can weld F,H & V Position.

3G PQR Will support only Vertical Welding.

If you need F&H position you need to establish New pqr with 2G position.

Regards,
Manikandan
9791367960






On Wed, Sep 1, 2021, 8:56 PM harenath jha <harenathjha@gmail.com> wrote:
Yes you can use it

On Wed, Sep 1, 2021, 17:20 DINESH KUMAR DEVENDHIRAN <dineshqc05@gmail.com> wrote:
Dear Experts
I need a clarification on AWS table 4.1 vs 4.10
As per table 4.1- for 3G position WPS shall be qualify for vertical position only
As per table 4.10 - for 3G position welder will qualify for Flat, Horizontal, vertical.

My doubt is if i have a WPS for 3G uphill position, can i use the same WPS for 1G&2G also ?
If not please explain.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/571704be-652c-417c-9c67-6400ec82034an%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPRS9UOScx2YEK2eVeOt%3D5PehBV3OtRdt%2B%2B_sB%2BaZu-JJGunaQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPdGVmODCwwk6ZLLcn%2BdxYATY49kaZa5RYtJn10iHwKq4du5bg%40mail.gmail.com.

Re: [MW:32504] AWS WPS & WELDER QUALIFICATION

Yes you can use it

On Wed, Sep 1, 2021, 17:20 DINESH KUMAR DEVENDHIRAN <dineshqc05@gmail.com> wrote:
Dear Experts
I need a clarification on AWS table 4.1 vs 4.10
As per table 4.1- for 3G position WPS shall be qualify for vertical position only
As per table 4.10 - for 3G position welder will qualify for Flat, Horizontal, vertical.

My doubt is if i have a WPS for 3G uphill position, can i use the same WPS for 1G&2G also ?
If not please explain.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/571704be-652c-417c-9c67-6400ec82034an%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPRS9UOScx2YEK2eVeOt%3D5PehBV3OtRdt%2B%2B_sB%2BaZu-JJGunaQ%40mail.gmail.com.

Re: [MW:32502] Welding process and NDT method for fillet welding

Magnetic Particle Testing (Wet ) or Dye Pen 

Thank you, 

Regards, 
S.SENTHILKUMAR


On Wednesday, 1 September, 2021, 08:36:00 am IST, Chiranjeevi A <chiranjeevipuvvula@gmail.com> wrote:



Dear Experts,

 

Please advice on NDT methods for fillet welding in plate welding (A36 mtl) for Ducts



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0xCpJmaGRR8QbY6JihPBAQbNDab%3D9Z%2BKqykWswmwNRZAg%40mail.gmail.com.

[MW:32501] Welding process and NDT method for fillet welding


Dear Experts,

 

Please advice on NDT methods for fillet welding in plate welding (A36 mtl) for Ducts



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0xCpJmaGRR8QbY6JihPBAQbNDab%3D9Z%2BKqykWswmwNRZAg%40mail.gmail.com.

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...