Monday, July 26, 2021

Re: [MW:32461] HARDNESS TEST

Dear Noel,
Greetings!
Can you send the exact excerpt clauses from Client specification regarding hardness test.

Kind Regards

On Monday, July 26, 2021, 07:14:35 AM GMT+3, Noel Tanilon <noel.tanilon@aboitiz.com> wrote:


Our Client is requesting hardness testing as mentioned in the equipment welding specification, where it stated the hardness test to be carried out on the following area for equipment which include tanks: 1. On Circumferential seam (some percentage) 2. Longitude seam (some percentage) 3. All temporary weld made and remove (100%) All the above requirements are so impractical to us since we are fabricating/erecting atmospheric tank (large diameters too). The amount of temporary weld (for erection purpose) are tremendous i.e. thousands for each crude oil storage tanks and hundreds on the miscellaneous tanks. The hardness test was carried out during the qualification of Welding Procedure Qualification and it meets the hardness value requirement. And there are no requirements for hardness tests as per API 650. I believe that it is meant for pressure vessel tanks only, but OWNER insists on the test since it is stated in the specification. Any comment on this client requirement? Please help.

Regards,

Noel
Noel C. Tanilon Jr
QA/QC Supervisor
Aboitiz Construction, Inc.
t 63 32 411 1800
m +63 917 849 8183
The information contained in this email message is intended for use only by the individual or entity to which it is addressed, and such information may be privileged, confidential and/or proprietary, and protected under applicable laws. 

Read about the full Aboitiz Disclaimer ( http://www.aboitiz.com/disclaimer)

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANff5sX-CKUrYid-4at6bYtKNN0SFLrsg%2Bw3kKfWK-uV4RdkEw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...