DEAR EXPERT
I am searching for welding consumables as per below requirement  for cryogenic vessel MDMT -196⁰ C 
Base material- SA 240 TYP 201LN.( UTS 655N/mm².
Imapct test- (-196⁰c,LE must be 0.38 mm,energy 34J.
Bend test at 4t,180⁰.
Previously I welded this material by Ni Cr Mo-3 filler wire and flux from a reputed manufacturer and result was acceptable all marine class surveyor.
At persent I am looking for  any alternative consumables which satisfy above requirements and cheaper than Ni Cr MO-3.
As required quantity is huge so I can go with unassigned welding consuambles also.

Guidance  regarding consuambles is highly appreciated.

Regards
Atul jha .
Mob no- 8817536323.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC1tTUJyNk7M0D19NgFbCegobKGxX%3DdamKtkZ49EiwgVszVcMA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3PODoZ3BpBygAWejFdCR98-JMAiOgW%2BU-w2r15BprCB8Q%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...