Sunday, July 11, 2021

[MW:32444] Defects in welding

Dear Experts,

We are facing defects in the stainless steel welding as per attached images, kindly let me know what could be the reason. 

Please note below information,

Consumable type: SMAW
Grade:E309LT1-1
Base metal: E309L plate
Co2 gas flow: 15-18
V: 28V
Current: 180-200 amps

Same batch of flux cored wire E309LT1-1 has worked just fine on the other jobs with similar applications. 

Thanks in advance. 

Regards, 
--
--
 
Aditya Gujar

---

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB89cpD8ioE8j-dUpwY4F7%3DLm0nDmB51tPLmongiwMG%2B0DvPzw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...