Dear Mr. Pushpraj,

Since ASME & TEMA does not specifiy tube wall thickness reduction limit, for C.S. materials 8-10% thinning is recommended as per Good Engg. Practice and reputed PMC spec.

Thanks & regards,

C. R. GANDHI


From: Madhan S <madhan0890@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Tuesday, November 17, 2015 9:11 AM
Subject: [MW:23889] Re: Allowable Tube Wall Reduction Tube-to-Tubesheet Joints expended in 2 grooves and seal welded

Dear Pushpraj

Formula for tube expansion, D=d+e+t

D- Tube ID after expansion.
d- Tube ID before expansion.
e- Clearance between tube OD and Plate ID
t- Applied Diameter expansion is 0.6 mm. (0..6mm Use can change depending on your groove depth.)

In your case you have seal welding also. So Don't worry for leakage.

With Regards,
Madhan. S




On Monday, November 16, 2015 at 7:54:08 AM UTC+3, Anand wrote:
Dear experts
 Please let me know the Allowable Tube Wall Reduction Tube-to-Tubesheet Joints expended in 2 grooves and seal welded 

Tube is SA179 ,20 mm OD & 2 mm thick
Tube sheet SA299 Gr B , 20.20 +_ 0.05 mm hole dia with 2 grooves inside the hole 

Please also share the applicable clause of TEMA or ASME stand.

Regards
Pushpraj Anand
  
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/80f9e288-02b6-4df8-beab-762d5de20648%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...