Re: [MW:23899] Other Project PQR Can be used New project on Different Clients?

yes, it is not project specific. Each organization (Contractor) shall be required to prepare a procedure qualification record

On 18 November 2015 at 21:43, dominic v.k.dominic <v.k.dominic@gmail.com> wrote:
Dear Expertise,
The contractor submitted other project PQR and approved by some other third party company and client.
My Question: Can used other client approved PQR for this new project and new Client?
In the code (API-1104 and ASME Section -IX) anywhere specified in this matter for Employer can be used other project PQR-If matching According the codes and new client requirements.
If yes, please provide code reference.

Thanks in Advance.
Best Regards,
Dominic.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubnyZ%3D1x-Hn2vaF84StPPu8Ms27HGPbDV_dn6smG%2BSySow%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...