[MW:23903] RE: 23902] Re: Other Project PQR Can be used New project on Different Clients?

Hi Dominic,

 

I would think there is some confusion in asking the question. My rationale to this issue is as follows:-

 

  1. There‘s no point in approving the PQR alone. A PQR doesn’t does serve any purpose without an approved WPS and vice versa.
  2. A PQR approved for one project meeting ASME Sec-IX requirements is perfectly O.K for other projects provided, procedure qualifications regime is ASME Sec-IX. Same is true for API 1104.
  3. However if additional requirements, e.g. different/various clients technical specifications are involved then new PQR may be insisted by project/contract requirements.  For example a PQR qualified to ASME Sec-IX+ Aramco Spec(Example Only)  may not be  approved  to ASME Sec-IX+ Shell’s Spec.

 

So the answer to your issue should be:-

 

  • It would be WPS+PQR which have to be reviewed by the client.
  • If the  welding qualification codes is API 1104 or ASME Sec-IX, there’s none specified in these codes that PQR approved for  project  X can’t be used project Y
  • However if there’re additional test mandated by client/project specifications, then new PQR qualification and approval of a new WPS is mandatory.

 

 

Thanks.

 

 

Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Engineering Specialist
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299

pgoswami@quickclic.net

pradip.goswami@gmail.com

All provided answer are personal opinions or personal judgements only. It's not connected with any employers by any means. 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Sundar Kumar
Sent: Thursday, November 19, 2015 8:00 AM
To: Materials & Welding
Subject: [MW:23902] Re: Other Project PQR Can be used New project on Different Clients?



On Thursday, November 19, 2015 at 6:50:01 AM UTC+3, dominic v.k.dominic wrote:

Dear Expertise,

The contractor submitted other project PQR and approved by some other third party company and client.

My Question: Can used other client approved PQR for this new project and new Client?

In the code (API-1104 and ASME Section -IX) anywhere specified in this matter for Employer can be used other project PQR-If matching According the codes and new client requirements.

If yes, please provide code reference.

 

Thanks in Advance.

Best Regards,

Dominic.

 

 

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9129bd1f-1407-46f3-9799-5f1c37e5fc94%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...