Monday, November 30, 2015

[MW:23935] Re: Bulge P-91 Pipe after PWHT

This bulging is due to restricted movement of the parts being post weld heated during PWHT .
Due to restraints at the end of the  pipes, the bulging might have taken place.
Also pl note  that PWHT temperature is a bit high ie 750 - 760 Deg C for GR 91   as compare of GR 22 , GR 11 ETC

On Tuesday, November 24, 2015 at 2:07:20 PM UTC+5:30, pradipsil wrote:
Dear Expert,
In P91 Material ( HRSG header Joint ) after pwht one joint is bulge.We did  Preheating ,Welding , Post Heating,& PWHT in proper way.
Can anybody explain why this bulge occurs & remedy.
During fit-up inspection & weld visual inspection all round the joint is perfect but after PWHT pipe is bulge 140 mm away from the   weld ment
Pic Attached
Regards,
Pradip

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f971b1aa-d3d4-43cc-974e-8cbf851ac79a%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...