In first step, engineers should investigate and analyse the effect of such cracks in a complete manner. Certainly it needs the complete package of data about observed cracks and their characteristics and effects.
--
-- The decision of using those materials with or without any reinforcement is not a concern of En 10163. You have to enter the world of FFS (Fitness For Service).
On Wed, Jun 17, 2015 at 8:15 PM, Mehdi Vafakhah <mehdi.vafakhah@gmail.com> wrote:
Dear Mr. shokriYou received this message because you are subscribed to the Google Groups "Materials & Welding" group.
Thank you for your reply . I prepared the repair procedure according to En 10163 but because of high volume of surface cracks ( in all over the angle surface ) its not possible to use it.
Is it possible to welding a reinforcing bare in such a surface condition without removing of cracks ?
According to aws d1.1 Engineer can permit it ?
On Wednesday, June 17, 2015 at 6:29:57 PM UTC+4:30, meisam shokri arfaei wrote:Please see EN 10025-2, 7.5.3. It will refer you to the EN 10163-1 to 3 for permissible surface discontinuity and repair modes.RegardsOn Wed, Jun 17, 2015 at 2:18 AM, Mehdi Vafakhah <mehdi.v...@gmail.com> wrote:--Dear expert,I'm recently working in a structural project as welding qc . During fabrication inspection, surface crack was found in angles material used in project ( as bracing ) so i reviewed the mechanical examination reports ( the tests are done according to En iso 10025-2 ) but absolutely mechanical properties and chemical analysis is ok! and that is so interesting to me .And after that according to the material examination reports, welding of a reinforcing bare is permitted by the engineer and its more interesting issue for me!However my question is according to any fabrication standard is it possible to welding on a cracked surface material like that ?(the depth of cracks are 3 mm in both sides and in all over the angles surface area .)Thank you.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/58e4afce-c563-45d9-baa3-c7c86243d959%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/152ef922-35b4-4a29-9dfa-66521b6535ec%40googlegroups.com.
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer
Tel.: +98 21 66282127
Fax: +98 21 66282779
Mob.:+98 912 1394023
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC8uMtu4QK5otOMOqVrZhBPKhrZcceZsDw9HYRVDMfqCL4t6nA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.