Thursday, June 25, 2015

[MW:23116] qualify WPS AWS D1.1

Dear all experts, please help me,

if I qualify WPS AWS D1.1 as picture :
A & B are the test piece cut from the spiral pipe, all are SAW process.example: t=12mm, OD = 800mm, 
my question is: according to table 4.2 AWS D1.1, the test piece B should be qualified for steel plate welding process,and range qualify will be 3mm to 2T, is it right?
also,according to AWS D1.1, the test piece A ( joint two pipes) is qualify for pipe and tubing, and range qualified is T/2 to 2T, is it right?

Thanks all .




--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8fdb75be-fa56-48d9-b4ff-e1620be76af5%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...