Thursday, June 11, 2015

Re: [MW:23067] WPS & PQR as per B31.12

Refer GR3, if you have IP follow ASME Sex IX, else for PL, use API 1104

On 11 June 2015 at 10:03, Siva Chidambaram <mechsivachidambaram@gmail.com> wrote:
Hi,
 
Whether any body can share me about the WPS & PQR requirements as per ASME B31.12.
 
Thanks and regards
M.Sivachidambaram
QHSE ENGINEER
GATES ENGINEEING & SERVICES


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubmDqFhQdjXBde%3Dheh5NG_3bGQ68RK_y5q88TbLui6YfRQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...