[MW:23058] RE: 23057] Weldability of API 5L and P355 NL1

Hi Raouf,

 

EN 10028:3, P355 NL1 is equivalent to ASME/ASTM SA/A516.

Chemical composition: (maximum permitted)

C           Si     Mn          P           S           Al               N           Cr

0.18     0.5   1.1-1.7    0.025   0.008   0.02min      0.012     0.3

 

Cheers

H.V.D

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com]
Sent: 02 June, 2015 8:12 PM
To: Materials-welding
Subject: [MW:23057] Weldability of API 5L and P355 NL1

 

Dear expert ,

 

We have to weld API 5L Gr X 60 with P355 NL1, our client is asking of the weldablity of this two materials .

 

I'm trying to find ASME equivalent for P 355 NL1 but without results.

 

Regards

 

SALHI Raouf

QA/QC Engineer

 

Tel: Morocco +212628979891

      Tunisia +21621458258

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1918751175.5427834.1433250720453.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...