Design Code : ASME Sec I, API 560 & API 530
Service: Non Corrosive.
We have CS tubes in the convection section (BFW service) of furnace and we are planning to operate during the emergency shut down (plant black out) for short duration of about an hour at higher temperature then the design temp. (425° C).
At this short duration of time the water tubes is going to see the no BFW flow condition (DRY).
Query: What is the max. temperature attainable (intermittent - 01 hour) by CS tubes (to avoid creep rupture). How much the temperature above the design temperature (425° C) can the CS tube be pushed for this short operation of time (01 hour)?
Regds/Jignesh
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Comments