[MW:21999] Plasma Powder form - ASME Sec.IIC not covered

Dear Experts,
 
 
ASME Sec. IX talks about Plasma welding process which use Powder as the filler metal product form.
Where as when I refer to ASME Sec.IIC, this powder form is not classified.
SFA 5.21 is

" SPECIFICATION FOR BARE ELECTRODES AND RODS FOR SURFACING"

Can you please advise, whether I can classify this powder in SFA 5.21 and prepare WPS, else this becomes my special variable.

Is there any new edition in ASME Sec.IIC which says about Powder form?

Regards

Vadivel M

07829007400

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...