[MW:22016] RE: 22011] CS Pipe API5L / A106 GR.B/X42 P2 (PSL2) instead of API5L / A106 GR.B/X42 (PSL1)
PSL 2 is a higher quality standard than PSL and few clients would object to received PSL 2 in lieu of PSL1. However you need to declare to your client what you are providing. The leaner chemistry of PSL 2 could give strength issues if anyone were to make pipe bends by induction bending from the material.
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Nirav Sanghavi
Sent: 29 September 2014 12:02
To: materials-welding@googlegroups.com
Subject: [MW:22011] CS Pipe API5L / A106 GR.B/X42 P2 (PSL2) instead of API5L / A106 GR.B/X42 (PSL1)
Can we supply Carbon Steel Seamless Pipe API5L / A106 GR.B/X42 P2 (PSL2) instead of API5L / A106 GR.B/X42 (PSL1)
Looking forward to your guidance.
Thanks
Nirav
M:+971(0) 50 9156242
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Comments