Tuesday, May 20, 2008

[MW:785] Re: Inch DIA

The term Inch Dia OR Dia Inch is used for the quantity of welding for the piping fabrication.
 
1 inch dia/Dia inch = Size of the joint X No. of the joints.
 
Regds/Jignesh
-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com]On Behalf Of Zameer Mohammed
Sent: Monday, May 19, 2008 6:14 PM
To: materials-welding@googlegroups.com
Subject: ***SPAM*** [MW:784] Inch DIA

Dear Friends,

 

What is the difference between 1 inch welding and 1 inch dia welding?

 

1 inch dia = 1* 3.14 = 3.14 inch. Is this right.

 

One full welding on a 42'' pipe is 42'' dia welding...is it right.

 

Thank you,

 

Regards,

 

Sabir

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

2 comments:

Unknown said...

What is the difference between 1 inch welding and 1 inch dia welding?

1 inch dia = 1* 3.14 = 3.14 inch.
Answer: this is the circumference of a 1" diameter pipe.

One full welding on a 42"pipe is 42"dia welding.
Answer: this is what you call inch-dia or dia-inch in pipe welding production or pipe erection term

Unknown said...

What is the difference between 1 inch welding and 1 inch dia welding?

1 inch dia = 1* 3.14 = 3.14 inch.

Answer: 3.14 inch in the above calculation is the circumference of a 1" diameter pipe.

One full welding on a 42" pipe is 42" dia welding
Answer: This is the inch-dia that is normally used for measuring a piping job, common in pipe welding production or pipe erection