Re: [MW:35869] 347H material weldability

What is service temperature of the equipment ?
If Ferrite number is to be controlled,  then TYP 16-8-2 filler metal is required as it has very low FN .
Check with designer/ Specs/ service experience 

On Sat, 25 Oct 2025 at 9:12 PM, Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
used in high temp superheater coils. No welding issues. may not get matching wire like ER 347H,E347H, instead u can use 347
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015, ISO 3834, EN 15085, 
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Sat, Oct 25, 2025 at 1:05 AM 'Rajnish Dixit' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Hi Zakaria,
Hope it is piping material and generally we use GTAW + SMAW welding processes to weld such stabilized grade material.

For SS347H material, the recommended welding consumables are AWS ER347 for Gas Tungsten Arc Welding (GTAW) and AWS E347 for Shielded Metal Arc Welding (SMAW).

Please check your customer's specifications for PWHT and other requirements. Being stabilized grade PWHT is recommended at 900 deg. cent. temperature for 4 hours.

Thanks,
Best Regards,
Rajnish 

On Tue, 12 Aug 2025 at 13:02, Zakaria ghrab

Hi experts,

I'm need information about 347H material weldability ( welding process, rod/electrode, temperature control, pwht, impact test?!, ....)
Could you help me with references please.


Thank you very much.





Thanks and Regards, 
-----
زكرياء غراب
GHRAB Zakaria 
Tunisia : +216 96 635 805
Bénin : +229 97 128 387


Yesterday is the past, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!

Le lun. 11 août 2025, 07:53, Kannayeram Gnanapandithan <kgpandithan@gmail.com> a écrit :
  Interpretation #: BPV IX-18-34
 Record Number: 18-771
 Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for Impact Testing Standard Designation: BPV Section IX Par/Fig/Table: QW-401.1 and QW-403.6 Edition/ Addenda: 2017 

Background:
 A welding procedure qualification was performed on a 40 mm thick test coupon in 1G position by GTAW (10 mm) and SMAW (30 mm). Tension and bend tests were performed on the 40 mm plate. 

A second welding procedure qualification was performed on a 6 mm plate in 3G position by GTAW and only impact testing was performed. A third welding procedure qualification was performed on a 6 mm plate in 3G position by SMAW and only impact testing was performed. All of the essential variables remained the same except for the coupon thickness. 
Question: 
May the PQRs listed above, support a WPS (GTAW+SMAW) for material requiring notch toughness with a qualified base material thickness range of 5 mm to 200 mm, GTAW weld metal thickness range 20 mm max. and SMAW weld metal thickness range up to 200 mm max.? 

Reply: Yes.   

 My queries .   Is it in order

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015, ISO 3834, EN 15085, 
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNVH-y4bk1Nw7_mw9GWJVWjuphN54KPtJrfAgwx%3DBthxg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAD8EeB2Qeq4qeeV4V5T2AkSsq55EZH8-0rv%3D1%2BLbksdB112L5A%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1091900790.162442.1761312265505%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eP3HmDzBma9Dy1%3Dk8UeUzeP3D8mfohCzWGYExcaLqzj0A%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CADder3MDgvQsb2gzUWK8fm_%2BKVVH9fWz0sCQ1mRE8_AxqA8Cvw%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...