In QW 202.4 dissimilar base metal thickness.
There is a two conditions ,one is 6mm or grater another 38mm or grater.
Based on P number we have to choose WPS for branch welds.
For butt welds L seam, C seam in thicker material will do tapering, in this condition thinner material thickness we will take for WPS selection.
QW-403-16 for set in ,set on joints pipe OD details given.
Sent from Outlook for Android
From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> on behalf of Anandhapadmanabha pillaim <anandhapadmanabhapillaim1997@gmail.com>
Sent: Sunday, October 19, 2025 9:14:31 PM
To: materials-welding@googlegroups.com <materials-welding@googlegroups.com>
Subject: Re: [MW:35847] SET ON ASME SEC IX
Sent: Sunday, October 19, 2025 9:14:31 PM
To: materials-welding@googlegroups.com <materials-welding@googlegroups.com>
Subject: Re: [MW:35847] SET ON ASME SEC IX
While considering the thickness, if it's a dissimilar thickness, the thickness of the smaller one and upper one should fall as per QW-451.1 if the qualification is made on a 38mm thickness coupon, the upper limit you will get unlimited still the lower one should fall within the WPS or you can combine 2 PQR and make one WPS inoder ro cover upper as well as lower limit.
On Sat, 18 Oct 2025, 11:41 am Elavarasan Mech, <elavarasan1861994@gmail.com> wrote:
Dear AllAs per ASME SEC IX Nozzle branch connection Set on which thicknesss consider for ( Nozzle or main pipe)WPS & WQT selection--
RegardsELAVARASAN
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4ym7crHij%3DVpKu%3DGgwWENPN1j1fR%2BhZyZZGCC2-OkgTFWQ%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ90KGSi2h8qWUABXqR-oC4dsov%3D8R6sTR5KXE8cQ9Fz14aPpw%40mail.gmail.com.
Comments