For set on joint branch pipe thickness should be taken for WPS. For WPQ branch OD and thickness essential variable.
Regards
D.V.Reddy
Sent from Outlook for Android
From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> on behalf of Elavarasan Mech <elavarasan1861994@gmail.com>
Sent: Saturday, October 18, 2025 7:51:28 AM
To: materials-welding@googlegroups.com <materials-welding@googlegroups.com>
Subject: [MW:35841] SET ON ASME SEC IX
Sent: Saturday, October 18, 2025 7:51:28 AM
To: materials-welding@googlegroups.com <materials-welding@googlegroups.com>
Subject: [MW:35841] SET ON ASME SEC IX
Dear All
As per ASME SEC IX Nozzle branch connection Set on which thicknesss consider for ( Nozzle or main pipe)WPS & WQT selection
Regards
ELAVARASAN
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4ym7crHij%3DVpKu%3DGgwWENPN1j1fR%2BhZyZZGCC2-OkgTFWQ%40mail.gmail.com.
Comments