Re: [MW:35655] Clarification Required on Welder Qualification – P-No. 8 vs. P-No. 45 (ASME Section IX)

A welder qualified using the GTAW process on P-No. 8 material is generally permitted to weld P-No. 45 material without a separate 

qualification, provided no essential variables have changed. This allowance is based on the grouping of base metals into P-Numbers 

in ASME Section IX, which groups similar materials so that qualification on one material covers others in the same group or related groups.

 

·   Table QW-423 in ASME Section IX lists base metals by their P-numbers and groups them into rows. This table defines which materials 

    can be considered equivalent for welder qualification purposes. If a welder is qualified on a base metal in a given row, they are qualified 

    to weld other base metals in the same row without requalification. 

Hence,

·    Welder qualified on GTAW P-No. 8 → permitted to weld P-No. 45 without requalification, if the filler metal (F-No.) is the same.

·     No changes in essential variables such as joint design, backing, thickness, welding position, or process.

·    The QW-423 table in ASME Section IX governs this equivalency and substitution of base metals for welder qualification.


This approach streamlines welder qualification by grouping similar materials and avoiding redundant testing while ensuring weld quality and 

code compliance. 

C Sridhar.


 

 

 



On Thu, 29 May 2025 at 21:41, venkateswara reddy Desireddy <dvreddy82@gmail.com> wrote:
No need new qualification. Please let me why new qualification required?

On Thu, 29 May 2025, 4:09 pm Vishwas Keskar, <vvkeskar123@gmail.com> wrote:
New qualification is required 
Sent from my iPhone

On 29 May 2025, at 11:47 AM, Karuppa Samy <samyqc08@gmail.com> wrote:


Hello Everyone,

I would like to clarify whether a welder who is qualified using the GTAW process on P-No. 8 material is also permitted to weld P-No. 45 material, or if a separate qualification is required for P-No. 45.

Additionally, I would appreciate it if someone could provide a brief explanation regarding the relevant table in ASME Section IX that addresses this qualification range.

Your expert input on this matter would be highly appreciated.



<image.png>


Regards,
K. Karuppasamy


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJg1SznAZ74w2eF6jFi5ZU%2Bmmu%3DYq5v35c86CyCWB%3Dy6HZ7RKQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/3775241C-7D39-4215-97C4-C9151BAB5652%40gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAEabyKmQPJ_RzZoPWeKE68%3D%2B8gNxi1L_koGC46fZW5uJtse%2B-Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHo%3DYiidCRJu4X9Ecy9DyyEsWDV6WH6cSsOpz-G%2B7624-nVESQ%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...