Hi,
Please share the information about reinforcement pad requirements against the ASME B31.3
Regards
Manish Kumar
Inspection(Mechanical) Engineer
On Thu, 29 May, 2025, 6:18 pm Tajuddin Mohammed, <tajuddinjntu@gmail.com> wrote:
as per 01-SAMSS-010 para 5.5 Reinforcing and Attachments
Steel plate used for reinforcing pads, sleeves, saddles and other structural
attachments shall conform to a code listed plate material with specified
minimum yield strength of 241.3 MPa (35,000 psi) or greater, depending on
design requirements.
All reinforcing and attachment welds shall be continuous. Skip or stitch
welding is not permittedOn Thu, May 29, 2025 at 2:17 PM Manish Kumar <mkmkr431@gmail.com> wrote:--Hi,Please share the selection criteria about the requirements of reinforcement pad of pipe.ThanksRegardsManish KumarInspection(Mechanical) Engineer
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHfQ4k5kqrtdmDSotHHzH2%2B5yS75a9zOJ6O7cPjtS3YnzFBYbg%40mail.gmail.com.
----Thanks & RegardsMohammed TajuddinWELDING INSPECTOR CSWIP 3.1Contact 0530833486JUBAIL
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CACZrEUYQ-0Bhme4752VFXbv1aKWcL1EzO%3DYGYaO_V%2B%2Bt-uBztw%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHfQ4k7bm1aViaeKb5QU1ayOSOtt2mYnKaX%3DWa2%3Dbf_2YtCnvA%40mail.gmail.com.
Comments