Hi, 

I hope you are all very well.
I wanted to know the reason behind why we use inconnect and E309L electrodes for buttering? what is the reason behind using those? Suppose a dissimilar weld between low alloy and carbon steel. We do buttering of inconnel on Low alloy metal.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABXHva58aooZKFhCva87G9aSjuKdbvAOH%3DGP_7%2BJb8TnPaHN4Q%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...