Saturday, July 6, 2024

[MW:35106] Re: Porosity Problem in Monel 400 Electrode ENiCu7

For such issue Electrodes with low hydrogen content ENiCu-7 are typically recommended for welding nickel copper alloys like Monel.
Hope you have taken care basic things of baking of electrode, Cleanliness, Welding parameters.

Regards,
Pravin Nimbalkar


On Friday, June 14, 2024 at 4:28:51 PM UTC+5:30 PSS wrote:
Please provide the solution for Porosity problem in N04400 during SMAW welding with electrode of ENiCu7.

Thanks in advance.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4a9f67e5-ba64-45de-a648-32161ab1619fn%40googlegroups.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...