Re: [MW:35052] Issues related to PQR

Dear Quang,

Writing Welding Procedure Specifications (WPSs) based on previously available Procedure Qualification Records (PQRs) that lack complete Non-Destructive Testing (NDT), tensile, hardness, and toughness reports may not comply with standard practices and regulatory requirements. Here's a breakdown of the situation and the guidance you need:

Key Points to Consider

  1. PQR Completeness:

    • The PQR must be comprehensive and include detailed reports of all required tests (NDT, tensile, hardness, and toughness).
    • The summarized PQR sheet, even if signed by relevant parties, is not a substitute for the complete documentation.
  2. Code and Standard Compliance:

    • Standards such as the American Welding Society (AWS) D1.1 and the American Society of Mechanical Engineers (ASME) Section IX specify the requirements for WPS and PQR documentation.
    • These standards mandate complete records of all testing conducted to qualify the welding procedure.

Issues with Incomplete PQRs

  • Verification:

    • Complete test records are necessary to verify the qualification of the welding procedure. Without these records, it's challenging to ensure that the procedure meets the required standards and specifications.
  • Audits and Inspections:

    • Incomplete documentation can lead to issues during audits and inspections by regulatory bodies or clients, potentially resulting in non-compliance findings.

Specific Standards and Documentation

  • AWS D1.1 (Structural Welding Code – Steel):

    • Section 4.9.3 requires that the PQR include records of all tests conducted to qualify the procedure.
    • A WPS derived from an incomplete PQR would not meet AWS D1.1 requirements.
  • ASME Section IX (Welding, Brazing, and Fusing Qualifications):

    • QW-200.2 outlines the requirements for the PQR, including detailed reports of all tests.
    • According to QW-201, a WPS must be based on a PQR that documents all required tests in detail.

Recommendations

  1. Complete the PQR Documentation:

    • Ensure that all missing NDT, tensile, hardness, and toughness test reports are attached to the PQR.
    • If necessary, re-perform the tests to obtain the required documentation.
  2. Consult Relevant Standards:

    • Review AWS D1.1 and ASME Section IX to ensure full compliance with all documentation requirements.
  3. Seek Expert Consultation:

    • Engage with welding engineers or certification bodies to validate the completeness of your PQRs and the adequacy of your WPSs.

Conclusion

Writing a WPS from an incomplete PQR is not compliant with standard practices and regulatory requirements. It is essential to have complete documentation, including all test reports, attached to the PQR. This ensures the validity of the WPS and compliance with standards such as AWS D1.1 and ASME Section IX.

If you need specific documentation references, the following sections from the standards will be useful:

  • AWS D1.1: 4.9.3
  • ASME Section IX: QW-200.2, QW-201

Ensure that your PQRs are fully documented before proceeding to write WPSs to avoid non-compliance and potential issues during audits or inspections.


On Wed, 5 Jun 2024 at 09:41, Dương Vinh Quang <duongvinhquanga13@gmail.com> wrote:
Dear experts, 
I am in the following situation, please ask experts for support and advice. Currently, our company wants to write WPSs from previously available PQRs, but the previous PQRs did not have complete NDT, tensile, hardness, and toughness reports attached, but only one PQR sheet summarizing the That report (of course fully signed by all relevant parties, including third parties). The questions raised are as follows: 
1. Is it wrong if we write WPS since then? Any documents that show this is wrong, please provide me. 
Thank you all!

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/45d0c269-3b29-47de-924a-becd59891411n%40googlegroups.com.


--
Best regards,

Amol K.B
B.E(Mech), CSWIP 3.2.2, NACE CIP 1 & ASNT LII(4M)

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAADcG1oSGVzkBaLaDV3pJf62MU4Q4Cjh7JutGv%2BwPpzRiMU0TQ%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...