Tuesday, June 4, 2024

[MW:35049] Waspaloy weld macrostructure etchant

Dear all, 
 
I would like to ask you if you have any information on which etchant would be best to get the macrostructure of the weld metal deposit of Waspaloy (material spec attached).
 
We have already etched with Carapella (pic attached) but the result does not give us the information we need to see the weld runs (multi-layer weld).
 
Thanks in advance

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b71a091b-4e21-46a5-a7b4-f810358409cfn%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...