Re: [MW:34743] Request to suggest best welding electrode for SAE1018 to EN8

E-7018. Stick Electrode.

মঙ্গল, ৯ জানু, ২০২৪ তারিখে ২:১৪ PM টায় তারিখে M PRABAKARAN <pjkaran@gmail.com> লিখেছেন:
Dear Sir,

Request to suggest best welding electrode for SAE1018 to EN8.

Regards,
M.Prabakaran
Trichy-India

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3df42401-73ee-47a7-90d3-79039e1f39f4n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGhQL0k-9w_sAjEciPs7kn8KkWxSZHpOJWDNH%2BTL-6RbCeK0Lw%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...