Wednesday, January 10, 2024

[MW:34737] Re: Welding 2 different pipe grades together depending on API 1104


SAES-W-12
7.4.1 Procedures for API SPEC 5L Grade X65 or higher shall be qualified for each specific material grade, where each grade includes the equivalent flanges and fittings with same SMYS and similar CEq. Qualification on API SPEC 5L grade X65 shall also qualify all lower grades 0 (including Grade B) for both API STD 1104 and ASME SEC IX.
On Tuesday, January 9, 2024 at 3:03:02 PM UTC+3 dia shukr wrote:
Hi friends

I have an existing pipeline with qualified WPS#1(API 5L Grade X60 Thick. 12.7mm) and a new pipeline with qualified WPS#2(API 5L Grade X65 Thick.17.48mm).
My question is do I need a new qualification WPS or I can follow WPS#2??

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d39776f5-3ba0-4f2c-be32-93d8b6a464d4n%40googlegroups.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...