The thickness is 5.54 & 21.4

في الأحد، ٣١ كانون الأول ٢٠٢٣, ٠٦:٤٧ Vishwas Keskar <vvkeskar123@gmail.com> كتب:
What is thickness ??
Sent from my iPhone

On 30-Dec-2023, at 5:10 PM, dia shukr <diashukr@gmail.com> wrote:


Hi friends

I have pipe A333 Gr,6 with design minimum temperature (-10C).Will I need to do a toughness test??As you know, depending on table A-1 in ASME B31.3 the minimum temperature is (-50C).

Thanks every one

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHQEAU55%2BGZ4WKpR-QGS4jGEOAFmPCzzcSh-0Ry2YmPfoEw-xw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/C28BD71C-4439-448F-AE97-38FA4B4B5588%40gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHQEAU4RxbjDWYmg1xf6DOjAeNmeiVV-ERecRkHWpTxEwEpc6w%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...