There are some differences between Cast & Forged products.

CAST VALVE                                                                             FORGED VALVE
1. Castings are normally associated                                          1. Except Hot shortness not much defects in
    with defects and Inclusions which                                               Forgings which can be controlled.
     affect the Integrity of the valve

2.  Normally no Heat Treatment after castings                           2. Forgings receives Grain refining Heat 
                                                                                                        Treatment and better rpoperties.

3. No limitation on Sizes of Valves                                             3. Only smaller sizes mostly

4. Low cost                                                                                 4. Higher cost


RT is specified only to Cast valves because it is prone to Defects like Porosities & inclusion.

Thanks & Regards

J.Gerald Jayakumar



On Wednesday, 6 December, 2023 at 08:53:31 pm IST, nasrath ali <nasrathbinliyakath@gmail.com> wrote:


Dear All,

As per API 6D, testing for Valves, Code does not call for Radiography Testing for Forged Valves, whereas RT is mandatory for Cast Valves.

Kindly clarify the reason for not stipulating RT on Forged Valve

Thanks.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/31f196c7-0051-4151-ae91-b902c77f0789n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...