Re: [MW:33052] P11 material hardness value

Pls provide some additional details.
Hardness values obtained.
Base Pipe/ PQR / Production Hardness

Thanks & Regards

J.Gerald Jayakumar




On Monday, 25 April, 2022, 07:13:14 am GMT+4, Chiranjeevi A <chiranjeevipuvvula@gmail.com> wrote:


Dear experts,

We have an issue in the hardness value for P11 material of pipe.

If the value exceeds what are the matigations required.

Kindly advice

Thanks and Regards
chiranjeevi

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0y-8DmngFND-R1R%3D%2BYCoCDJURQwGOeA5Cb2M8HJAouxrw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...