Friday, April 1, 2022

Re: [MW:33013] Fwd: WPS TO QUALIFY THE OF THE WELDER

Hi,
As per Table QW451.4 All Groove weld test qualified for All fillet sizes on all base metal thicknesses and all diameters.


Thanks& Regards,

(Karthik)
Karthikeyan.S
M: +66-892512282


On Friday, April 1, 2022, 10:11:08 AM GMT+7, Rene Alvarado <rene.alvarado.lozano@gmail.com> wrote:


FE DE ERRATAS

 

Can I use a WPS qualified with the SMAW process in position 6G on pipes Copper Nickel to Carbon Steel with a thickness of 0.237" and with backing ring to qualify the skill of the welder in fillet welding with the SMAW process in position 5F on pipes Copper Nickel ( O.D. 2 ½" thickness 0.280") to Carbon Steel (O.D. 3" schedule 160 in accordance ASME IX?

 

Thanks

---------- Forwarded message ---------
De: Rene Alvarado <rene.alvarado.lozano@gmail.com>
Date: jue, 31 mar 2022 a la(s) 08:40
Subject: WPS TO QUALIFY THE OF THE WELDER
To: <materials-welding@googlegroups.com>


Experts

 

Can I use a WPS qualified with the SMAW process in position 6G on pipes Copper Nickel to Carbon Steel with a thickness of 0.237" and with backing ring to qualify the skill of the welder in fillet welding with the SMAW process in position 6G on pipes Copper Nickel to Carbon Steel with a thickness of 0.125"  ?

 

Thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CAHbC_j1M2mbAJbiCsAfyikj-CPst%2BEtPqr%3Dm9nA6Oh5Hg_tQkA%40mail.gmail.com
.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...