Re: [MW:32540] change in sfa number

There are 3 points to be considered as experts mentioned as below.

1. In ASME 2021 edition SFA 5.36 has been discontinued but I suppose the recalled may be used based provided the welding consumable certificate matches with A-Number of that Qualified for PQR.
 
2. Both SFA 5.20 & SFA 5.36 falls under F-Number 6 & hence  no issue.

3. Ensure the Shielding gas as qualified for 100%Co2

Thanks & Regards

J.Gerald Jayakumar



On Thursday, 30 September, 2021, 08:51:15 am IST, Chaudhary Zafar Iqbal <chzaiqbal88@gmail.com> wrote:


Hello good evening all experts
Can we use E71T1-1C-H4/H8 AWS SFA 5.36 filler wire instead of E71T1-1C-H4/H8 AWS SFA 5.20 if yes then please send me any  reference from code and standard by ASME-2C or SEX 9 or SAES- W12 or W11 or any international standard because our WPS is qualified on AWS 5.20 but we recieved Consumable material AWS SFA 5.36.         This attached label is recieved material 

Regards ,
Zafar 
00966544639978 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP9k9XfupDcLPwdc9kiJyUMxaU%2Bhz%3DHr13PVMmsgj_bO%3Dy_OEw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...