[MW:32528] Essential variables for Welding Procedure as per API 1104 22nd edition

Greetings,
As per Latest's edition of API 1104 (22nd edition) Table 1 Essential variables for qualification of welding procedure Specifications, Diameters are not listed as a essential variables.
Please share your experiences with standard references for diameter of Pipe are essential variables or not as per API 1104?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/C7F16A03-1358-4AE6-AD80-9A69B0878B61%40gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...