Dear friend ,
this may be related to high heat input especially the cracks location in photos mention the points of doubled heated times .
high temp. with Ni/Cu alloys make carbides precipitate easier leading to cracks also coarse grain size which increase with heat have more tendency to crack as precipitation area increase

Best Regards ,
AWS CWEng.   Ahmed Osman 

On Monday, August 30, 2021, 11:42:03 a.m. GMT+3, Jeya Prakash <jeyaprakashjj@gmail.com> wrote:


Dear Experts,
We are facing cracking issues during welding in Monel 400 Tube to Tubesheet Joints. Refer attached photographs.
Tube: SB-163 UNS-N04400; 25.0 mm OD x 2.0 mm thk
Tubesheets: SA-336M Gr F304L + SB-127 UNS-N04400 (48 + 10 mm thick clad)
Welding: ERNiCu-7 GTAW filler wire with Ar shielding gas.
crack locations: weld toe on tube side, tube ends.

Kindly share the reason for such cracking, and precautions required during Monel 400 welding.

Thanks in Advance.

Regards,
Jeya Prakash. J

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL5WJhc%2BRkjr6oAUNp8uvhCP1imK0on-mqp7jbWcVAZC0PRy-Q%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...