Monday, August 30, 2021

Re: [MW:32495] Cracking of Monel 400 TTS welds

over heated
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Mon, Aug 30, 2021 at 2:12 PM Jeya Prakash <jeyaprakashjj@gmail.com> wrote:
Dear Experts,
We are facing cracking issues during welding in Monel 400 Tube to Tubesheet Joints. Refer attached photographs.
Tube: SB-163 UNS-N04400; 25.0 mm OD x 2.0 mm thk
Tubesheets: SA-336M Gr F304L + SB-127 UNS-N04400 (48 + 10 mm thick clad)
Welding: ERNiCu-7 GTAW filler wire with Ar shielding gas.
crack locations: weld toe on tube side, tube ends.

Kindly share the reason for such cracking, and precautions required during Monel 400 welding.

Thanks in Advance.

Regards,
Jeya Prakash. J

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL5WJhc%2BRkjr6oAUNp8uvhCP1imK0on-mqp7jbWcVAZC0PRy-Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePsNtBe5EVUNT9cPt-vCOTUMWar3FeNZ_j56vHfAn58uA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...