based on toughness requirement
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE, CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer.
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349
On Fri, Feb 5, 2021 at 8:36 AM Chandru Sekar <chandruyou25@gmail.com> wrote:
Why they segregated as group and in which basis ?--On Thu, 4 Feb 2021, 08:31 Anban, <gane2478@hotmail.sg> wrote:Dear ExpertsNeed your guidance in understanding PWHT minimum Holding Time base material thk.-65 ~ 75mmP-No. 1, Group Nos. 1–3Minimum Holding Time at Temperature for Control Thickness [Note (2)]-Up to 50 mm (2 in.)-1 h/25 mm (1 hr/in.);15 min min.-Over 50 mm (2 in.)-2 hr plus 15 min for each additional 25 mm (in.)Best RegardsGanesan--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b538da9f-4e78-4b7c-85c3-7679328ed9bdn%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGWOcnqMNXcWFH-bUvTt7GM1yoJJC6o5fUR_aKy3aWTuQs5fPQ%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.