Monday, February 1, 2021

Re: [MW:31971] Re: SS 405 grains

Thank you for your answer. I was wondering what would happen to grains of stainless steel 405 grains as hanger in boiler  when they exposed to high temperature for long time?

On Sun, Jan 31, 2021 at 22:13 Vishwas Keskar Welding Manager WELDING <vvkeskar123@gmail.com> wrote:
These are straight Cr Stainless steels for high temperature application.
In boiler , you can use this material.
Pl. send what attachment part you are looking for ?


On Monday, January 25, 2021 at 7:42:58 AM UTC+4 Emad wrote:
Dear all,

what will happen to the grains of a ferritic stainless-steel type AISI 405 used as an attachment of a hanger bar in a boiler, when it is exposed to flame temperatures of the boiler for 4 years of continuous operation? It is understood that the 405 steel will not oxidize in the high-temperature service environment.

Regards,

Emad


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f2ee4edc-671c-4f44-82e8-092cf1fb1198n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABtwbJGCA85f3p-Wzj0nCv0O7Pigf8VMKXFkwtNR%3Dbga-0oKGw%40mail.gmail.com.