Hi

Required 3.1 certificate or coc as per client requiredment / mar / mr.

If 3.1 certificate is required, chemical and mechanical properties / values shall be indicated on the certificate along with pmi report.

Check also is there any external coating required as per client spec

Regards
Govindan

On Feb 29, 2016 2:00 PM, "Ludmila MANUEL" <ludmila.manuel@total.com> wrote:

 

 

Dear experts,

 

I need to procure this material

 

Hex Bolt & 2 nuts M20 x 75 based on ISO 3506-1 / A4-80 based on your experience, could you give me your feedback about material certificate, tests requirements and which I need to work with.

 

Thanks

 

ludmila

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1B0224B9A78AB34285E27B011195A046AA6F2F213E%40AOEPTTA-EG11.main.glb.corp.local.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANiuf9c-WoqXkja%3DU2SZ2Z02QO2CRamA%2BHcNrdystD-ZRuAx2w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35725] Dismillar material Welding

Dear experts,  In my Hydro Electric Project  materials using A517Gr.F and A537CL-II.  For A517Gr.F using E 11018M and A537CL-II using E 9018...