Dear Sir,
-- As per ASME B31.3, for branch connections, PWHT is to be done for the entire circumference of main pipe. Is there any exceptions/code interpretations for that, in Carbon steel material or Alloy steel material (SA335 Gr P9,95)?
For example: A 3/4" branch is done on the main pipe of 60" dia. As per the code requirement, the entire 60" dia is to be wrapped with coil and PWHT is to be done.
Thanks in advance.
Regards,
Hareesh K V
+91-8547859202
--
----------------------
Hareesh K V
+91-9447625012
Hareesh K V
+91-9447625012
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM3LgAWX5nLOPkVL5UxS5uRTSO%3DKj%3DuWk6bmYbmkkJO%2BnQMy_A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments