RT should be based on the customer requirements / ensure that the soundness of castings. Verification of your methoding process.
Sent from my Mi phone
On prashant pansare <prashant.pan17@gmail.com>, 13 Mar 2016 09:27 wrote:
-- --Dear All,Is ther any size restriction to carry out RT of cast body for Ball Valve (A 216 WCB).ASME B 16.34 does not mention size limitation for RT of Valve Body.--My vendor says that for 2" Ball Valve of A 216 WCB, RT is not required.Kindly suggest.Thanks & Regds,Prashant PansareCell no - 09987189854
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFw%3DPEj94BnimzQZ6VbS4ZstrsOB3n9s4nPDLLSBDARd71L3Wg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/r8sp5etf52qb382u8gljguof.1457858115336%40email.android.com.
For more options, visit https://groups.google.com/d/optout.
Comments