Wednesday, March 25, 2009

[MW:1805] RE: 1804] 410 weld overlay on SA 516 Gr 70

What are the welding parameters adopted, especially the preheat & PWHT?

High hardness values render the material prone to cracking during fabrication, the selection of appropriate preheating levels and welding procedures is critical to the success of the welding process.

Select consumable with lowest C content from the lots.

 

Recommended reading: D.N. Noble, "review of practices for welding type 410 stainless steel," Edison Welding Institute

 

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of JASPAL SINGH
Sent: Wednesday, March 25, 2009 2:22 PM
To: Materials & Welding
Subject: [MW:1804] 410 weld overlay on SA 516 Gr 70

 

 

Is it possible to clear the bend test in SS410 weld overlay. The

barrier layer is E309LMo .

if possible let me know how.

 

Jaspal Singh

919996624244

 

 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...